Question 1) If the decay is nearing pulp. What is the good base or liner used below amalgam.

Question 2) If the decay is nearing pulp. What is the good base or liner used below composite.

Question 3) If I need to apply desensitizing agent. What is the right way of applying desensitizing agent?

Please reply

Thanks.

ASB

Members don't see this ad.
 
http://www.youtube.com/watch?v=gb8Z7bTcLNo

copalite is the traditional varnish under alloys. dycal and vitrebond under composites.
Apply your desensitizer and then etch.(some stuff about smear layer being better removed so do it after, doesn't matter though.)
 